Home > Knowledge > Content
Brick drying and cooling
- Jul 26, 2018 -

Brick drying

The adobe after the press molding contains a certain amount of water, even if it is extremely small, it will affect the strength of the adobe. Therefore, the slab is then sent to the drying kiln for drying. After drying the brick, the moisture content has dropped from 7% to about 0.5%.

The length of the drying kiln determines the degree of moisture drying of the tiles. The ultra-long 320-meter roller road drying kiln can not only make the moisture content of the bricks less than 0.5%, but also does not deform when fired.

Brick cooling (surface cleaning)

The dried bricks are cooled and surface cleaned before proceeding to the next process.